With the increasing of mass fraction of PEG, membrane porosity and pure water flux become larger, and the maximum tensile strength and elongation at break of the membrane criterion decrease gradually.
随着PEG质量分数的增加,膜孔隙率与水通量变大,最大拉伸强度、断裂伸长率等力学性能逐渐减小。
The mass transfer coefficient was higher for the big porosity membrane than for the small porosity one at same experiment condition.
同一传质体系,在相同流动条件下孔隙率大的膜的传质系数大于孔隙率小的膜的传质系数。
A porous silk fibroin membrane could be prepared through freeze-drying process, with dense top surface, porous bottom surface in low porosity and porous inner portion in high porosity.
采用冷冻干燥法可以制得下表面为致密结构,上表面为孔隙率较小的多孔结构,而内部是孔隙率较大的多孔结构的丝素膜。